- Institution
- PI Photovoltaik-Institut Berlin AG (PI Berlin), accredited test laboratory (ISO 17025), as stated, Germany
- Equipment named
- Class AAA flasher Pasan SSIIIb
- Application
- STC I-V measurement of CdTe, CIGS and µc-Si thin-film modules from three PID-affected plants, before and after PID tests to IEC TS 62804-2 (85 °C, 85 % RH, maximum system voltage)
- Use
- Accredited testing
- Published uncertainty
- ±2.9% for single junction (CdTe and CIGS) and ±5% for double junction (µc-Si), coverage not stated
- Technologies
- Thin film, CdTe, CIGS, Degradation, Field-aged modules
- Topics
- Venue
- Photovoltaics International (PV-Tech technical paper), pp. 75-83, 2018
Significance
PI Berlin's ISO 17025 laboratory measured CdTe, CIGS and micromorph modules on a Pasan SSIIIb to quantify potential-induced degradation and recovery of thin-film plants.
From the source
“Before and after each exposure the IV curves have been recorded using a Class AAA flasher Pasan SSIIIb.”
This entry summarises a third-party publication. It does not imply that the institution or the authors endorse Pasan SA or its products.