The measurement problem
The efficiency of a perovskite device depends on scan rate, scan direction and what happened to it in the minutes before. Statistics on about 200 cells from 30 sources showed that conventional I-V scans give a usable open-circuit voltage but can widely misestimate short-circuit current and efficiency [1]. A pulsed flash of milliseconds, however long by silicon standards, is far shorter than these ionic time constants.
The physics behind it
- Ion migration and accumulation produce I-V hysteresis and reversible changes under light and in the dark, including fatigue over light-dark cycles [4].
- IEC TR 63228 lists the challenges of emerging PV: instability over time, unusual spectral responsivity, small device size, difficulty measuring temperature, transient response, optical interference and non-linear response to irradiance [5].
- Ultraviolet content of the light can assist decomposition for some architectures, so the spectrum of a stability test matters [4].
What the measurement must achieve
- Report the steady-state (stabilised) maximum power under continuous illumination, not only a scan-derived Pmax [2].
- Define the active area with an aperture mask, correct spectral mismatch and report preconditioning and scan conditions [3].
- Use a convergence criterion, for example a current change below 0.1 %/min at each voltage step, as applied by Fraunhofer ISE on a tandem module [6].
- Control and monitor device temperature during long exposures.
- For stability, follow and report an ISOS protocol (for example ISOS-L light soaking at defined temperature and load) [4].
Applicable standards
| Standard | What it governs here |
|---|---|
| IEC TR 63228:2019Measurement protocols for PV devices based on organic, dye-sensitized or perovskite materials | The IEC document on emerging PV measurement: a Technical Report listing the challenges, without consensus protocols. No later IEC specification on perovskite measurement was found (November 2026). |
| IEC 60904-1:2020Measurement of photovoltaic current-voltage characteristics | Clauses on stabilisation and equivalence to steady-state performance. |
| ISOS protocols (Khenkin et al., 2020)Consensus statement for stability assessment and reporting of perovskite photovoltaic devices | Community consensus protocols for stability testing and reporting (not a standard). |
| IEC 60904-7:2019Computation of the spectral mismatch correction | Spectral mismatch correction against the reference device. |
Measurement technologies: advantages and limitations
| Mode | Use | Limitation |
|---|---|---|
| Short or long xenon pulse | Voc screening, transient studies | Too short for the ionic steady state [1] |
| Multi-flash | Not a substitute for steady state | Each flash still far shorter than seconds-to-minutes time constants |
| Steady-state xenon or LED | Stabilised power, MPP tracking, preconditioning, ISOS-L | Heats the device; UV content matters for stability tests [4] |
Where Pasan equipment fits
- Nexun Perovskite (Avalon ST)The Nexun PRO or PRO Max of Pasan's sister company Avalon ST with the steady-state add-on: steady-state source over 300 to 1000 nm (1200 nm option), synchronised with the 500 ms pulse so the flash can fire during preconditioning.
- LED Light SoakerContinuous regulated LED light with MPP, Isc or Voc bias for light soaking full-size modules.
- Article: measuring perovskite and capacitive cellsPasan's article on the measurement problem.
Technical questions
- Why not report the efficiency from a fast J-V scan?
- Fast scans capture a non-steady state; on about 200 cells they gave a good Voc but widely misestimated Jsc and efficiency [1].
- What should be reported instead?
- The steady-state maximum power under continuous illumination [2], with the preconditioning and scan conditions stated.
- Is there an IEC standard for perovskite measurement?
- Only IEC TR 63228:2019, a Technical Report summarising challenges without consensus protocols [5].
- What is ISOS-L?
- The light-soaking family of the ISOS stability protocols: L-1 at ambient temperature, L-2 at 65 or 85 °C, L-3 adding about 50 % relative humidity [4].
- Can a long-pulse xenon simulator measure perovskite?
- It can screen Voc and study transients, but a stabilised power needs continuous light for seconds to minutes.
References
- , “How useful are conventional I-Vs for performance calibration of single- and two-junction perovskite solar cells?”, Solar RRL 6, 2100867, 2022. doi:10.1002/solr.202100867
- , “Metastability in performance measurements of perovskite PV devices: a systematic approach”, Journal of Physics: Energy 3, 021001, 2021. doi:10.1088/2515-7655/abd678
- , “Comprehensive performance calibration guidance for perovskites and other emerging solar cells”, Advanced Energy Materials 11, 2100728, 2021. doi:10.1002/aenm.202100728
- , “Consensus statement for stability assessment and reporting for perovskite photovoltaics based on ISOS procedures”, Nature Energy 5, 35-49, 2020. doi:10.1038/s41560-019-0529-5
- , “IEC TR 63228:2019, Measurement protocols for photovoltaic devices based on organic, dye-sensitized or perovskite materials”, International Electrotechnical Commission, 2019. Source
- , “Traceable efficiency determination of large-area perovskite on silicon tandem modules: insights from a calibration laboratory's perspective”, Progress in Photovoltaics 33, 815-827, 2025. doi:10.1002/pip.3928
How this page is written: claims about physics and standards cite published sources, claims about Pasan equipment repeat only what the product pages state, and no other manufacturer is named. Editorial method